Susan,
I did not receive the photo.
Debby
Trace Labs
-----Original Message-----
From: Susan Mansilla [mailto:[log in to unmask]]
Sent: Wednesday, February 12, 2003 11:48 AM
To: [log in to unmask]
Subject: Re: [IPC-600-6012] Zone Concept
The photo above - hopefully this will be accepted by the forum and not
stripped - presents a real problem and should be
considered by everyone when we decide where to draw that zone line. Using
the internals that extend the farthest plus
3 mils would allow complete voiding between layers 2 and the ground plane.
Susan