IPC-600-6012 Archives

October 2005

IPC-600-6012@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Scott Bowles <[log in to unmask]>
Reply To:
(Combined Forum of D-33a and 7-31a Subcommittees)
Date:
Thu, 13 Oct 2005 11:16:25 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (45 lines)
Constantino,
Do you consider these areas to be areas to be solder to or not to be
soldered to?  You may also want to consider paragraph 3.5.4.7 of IPC-6012B
regarding class and percentage allowable to have exposed copper.

Regards,
Scott A. Bowles
Director of Quality and Technology
Sovereign Circuits Inc.
12080 DeBartolo Drive
North Jackson, OH 44451

Phone: (330) 538-3900 x211
Fax:   (330) 538-2434
Cell:  (330) 717-2125
email: [log in to unmask]

-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]]On Behalf Of Constantino
J. Gonzalez
Sent: Thursday, October 13, 2005 10:46 AM
To: [log in to unmask]
Subject: [IPC-600-6012] Exposed Copper


Hello everybody, here are some photos, could you tell me if they comply with
IPC-A-600G? Also includes traces to SMT pads. I believe section 2.9.1 of the
600G covers the criteria......or not?


Regards

Constantino J. González
President / Consultant Engineer
IPC-A-610 Committee Chairman

ACME, Inc.
AMERICAN-HISPANIC COMPANY
513 CLEVELAND STREET
RAPID CITY, SOUTH DAKOTA 57701
USA
E-mail: [log in to unmask]
Phone: 605-381-5963
Fax:    605-341-4261

ATOM RSS1 RSS2