Thought for the day: as most lead-free alloys require higher soldering
temperatures, how much extra energy will be required? How much extra CO2
will this cause to be emitted? While doing the calculations, remember
that the losses of energy to the atmosphere from a low temp heat source
(ie <500°C) is roughly proportional to the square of the difference in
temperature between the source and the ambient air.
Brian