Under the code ENIG
Finish Electroless nickel 3 micrometers min all 3 classes
Finish Immersion gold .05 micrometers min all 3 classes
-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of
Smith, Donn
Sent: Wednesday, July 13, 2005 9:35 AM
To: [log in to unmask]
Subject: [DC] Plating thickness
I find that my set of IPC-2220 has become outdated (specifically 2221).
So that I don't have to wait until I can requisition and receive my new
set, may I impose on someone who already has the new version?
Referencing the Feb 1998 version of that document, Table 4-3 Final
Finish, Surface Plating Requirements (page 20):
Electroless Nickel 2.5 - 5.0 micrometers (across all three classes)
Immersion Gold 0.08 - 0.23 micrometers (across all three
classes)
Here's the question(s): Have either or both of those thicknesses
changed in the newer version (IPC-2221A)? If so, what are the new
values?
Thanks very much (in advance)!
Donn
Donn Smith, CID
Senior PCB Designer
GARMIN International
1200 E. 151st Street
Olathe, KS 66062
(913)397-8200
(913)397-8282 Fax
[log in to unmask]
www.garmin.com
-------------------------
This e-mail and any attachments may contain confidential material for
the sole use of the intended recipient. If you are not the intended
recipient, please be aware that any disclosure, copying, distribution or
use of this e-mail or any attachment is prohibited. If you have
received this e-mail in error, please contact the sender and delete all
copies.
Thank you for your cooperation
------------------------------------------------------------------------
---------
DesignerCouncil Mail List provided as a free service by IPC using
LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with
following text in the BODY (NOT the subject field): SIGNOFF
DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET
DesignerCouncil NOMAIL/(MAIL) Search previous postings at: www.ipc.org >
On-Line Resources & Databases > E-mail Archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
---------
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|
|
|