DESIGNERCOUNCIL Archives

August 2001

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Keach Sasamori <[log in to unmask]>
Reply To:
(Designers Council Forum)
Date:
Mon, 27 Aug 2001 13:42:44 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (29 lines)
Forwarding a posting for Andrew Brenner:

From: [log in to unmask]
Date: Mon, 27 Aug 2001 11:07:17 -0400
X-MIMETrack: Serialize by Router on CORLNM06/COR/PARKER(Release 5.07a |May
14, 2001) at
 08/27/2001 11:07:45 AM
MIME-Version: 1.0
Content-type: text/plain; charset=us-ascii

Using a thermode tip, I am attempting to bond a 37.5 gage electrical copper
wire to a phosphour bronze electrical pin .020" thick to the leg of an
axial diode.  I get what looks like a cold solder joint with out Flux, but
a good connection with Flux.  This three piece assembly will be placed in
plastic part made out of Liquid Crystal Polymer with 15% glass fill (LCP
15).  What happens to the LCP since if flux is used since the flux can not
be washed or cleaned off.  Will it corrode the LCP or would it eventually
fail itself?

---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To set a vacation stop for delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2