At 07:25 AM 4/1/96 -0500, Mark R. Peltier wrote:
> I have been using SMT for so long, I forgot the rule of thumb for
>determining the lead-lead spacing for axial leaded resistors. Isn't
>there an equation that is used? Any help would be appreciated. Thanks,
>
>Mark R. Peltier
>e-mail:[log in to unmask]
>
>
IPC-D-275 figure 4-9 states to ocmes out from the component body 2 diameters
but not less than 0.03 inch. to the biginning of the bend raduis. The bend
raduis is determined by the lead diameter. up to 0.030 inch, R = 0.030. From
0.030 to 0.047 inch, R = 1.5 diameters. Larger than 0.047 inch, R = 2 diameters.
Regards;
Gary Ferrari
Chairman - IPC-D-275
Regards,
Gary Ferrari
Tech Circuits
[log in to unmask]