Just curious....how does your contract manufacturer take to any traces under
0603 & 1206 resistors ??
Ours complains because of the risk of tomb-stoning when any feature, such as
silkscreen, vias, traces are under
these descretes .....again..." in search of an ideal world ".....
Regards
TDK
> -----Original Message-----
> From: Matthew Lamkin [mailto:[log in to unmask]]
> Sent: Wednesday, October 23, 2002 7:37 AM
> To: [log in to unmask]
> Subject: Re: [DC] SMT Jumpers
>
>
> As Don says, use zero ohm resistors, we use a 1206
> exclusively for "jumping"
> tracks, allowing 2 tracks through it, although if you want
> to jump more you should be able to get a larger size.
>
>
> > -----Original Message-----
> > From: Mark Mainland [SMTP:[log in to unmask]]
> > Sent: Wednesday, October 23, 2002 2:00 PM
> > To: [log in to unmask]
> > Subject: [DC] SMT Jumpers
> >
> > Hello,
> > I've got a board that needs to be routed on a single side,
> I'm looking for
> > some SMT jumpers that come on tape & reel. I have looked at
> Zierick but
> > they only have a .300" & 1.5" size, does anybody have a
> source that has
> > more sizes available?
> >
> > Thanks.
> >
> >
> >
> > Mark Mainland, C.I.D.
> > Sr. PCB Designer
> > Cherry Electrical Products
> > 3600 Sunset Ave.
> > Waukegan, IL 60087
> > PH: 847-662-9200 Ext. 3359
> > FAX: 847-360-3551
> > Pager: 888-819-0198
> >
> >
> --------------------------------------------------------------
> ------------
> > ------- DesignerCouncil Mail List provided as a free
> service by IPC using
> > LISTSERV 1.8d To unsubscribe, send a message to
> [log in to unmask] with
> > following text in the BODY (NOT the subject field): SIGNOFF
> > DesignerCouncil. To set a vacation stop for delivery of
> DesignerCouncil
> > send: SET DesignerCouncil NOMAIL Search previous postings
> at: www.ipc.org
> > > On-Line Resources & Databases > E-mail Archives Please
> visit IPC web
> > site http://www.ipc.org/html/forum.htm for additional
> information, or
> > contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> >
> --------------------------------------------------------------
> ------------
> > -------
>
> --------------------------------------------------------------
> -------------------
> DesignerCouncil Mail List provided as a free service by IPC
> using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with
> following text in
> the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
> To set a vacation stop for delivery of DesignerCouncil send:
> SET DesignerCouncil NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources
> & Databases > E-mail Archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm
> for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> --------------------------------------------------------------
> -------------------
>
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To set a vacation stop for delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|