Wanted to summarize the feedback I received from several fabricators.
Embedded capacitance is widely available. Standard core constructions of >=0.002" material between solid planes provide planar capacitance and do not add significant, if any, cost to the product. Specialized core materials <0.002" are available from a number of material vendors and are being offered by many fabricators.
Embedded resistance is not widely available, has a very limited range of actual values available, and is expensive to implement. It was suggested the technology was more applicable to specialized low volume applications than cost sensitive volume production.
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 16.0.
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|
|
|