I've heard of something called "Easy Hole" which is nickel holes in CEM3,
offered by a european company named Eurocir. Another european company,
BREE, offers something called "copper hole". As far as I know, these are
high volume, low density alternatives to FR-4, PTH. Hadn't heard of "silver
hole" before...
-Chris Ball
"Brooks,Bill"
<[log in to unmask] To: [log in to unmask]
OM> cc:
Sent by: Subject: Re: [DC] Silver through hole
DesignerCouncil technology
<DesignerCounci
[log in to unmask]>
02/05/02 02:24
PM
Please respond
to "(Designers
Council
Forum)"; Please
respond to
"Brooks,Bill"
Do you mean Pins thru paste? an assembly technique?
Not sure what silver thru hole is referring to...
-Bill Brooks
-----Original Message-----
From: jblier [mailto:[log in to unmask]]
Sent: Tuesday, February 05, 2002 8:17 AM
To: [log in to unmask]
Subject: [DC] Silver through hole technology
Hello!
I'm looking into something called silver through hole technology.
Could any of you give me inputs, opinions or personal experience with
this technology?
Is it any good or it's more trouble then it's worth?
Thanks,
--
Jimmy Blier
CAD Department. (Senior Cad Designer)
P A R A D O X
S E C U R I T Y S Y S T E M S
Email: [log in to unmask]
----------------------------------------------------------------------------
-----
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To set a vacation stop for delivery of DesignerCouncil send: SET
DesignerCouncil NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To set a vacation stop for delivery of DesignerCouncil send: SET
DesignerCouncil NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
"This e-mail message is intended only for the use of the named
recipient(s).
The information contained therein may be confidential or privileged, and
its
disclosure or reproduction is strictly prohibited. If you are not the named
recipient, please return it immediately to its sender at the above address
and destroy it."
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To set a vacation stop for delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|