I searched the several internet sites and couldn't find a standard that
covers the following question:
What is the MINIMUM pin length in order to be able to reliably solder a
through-hole component to the PWB?
The pin diameter is 25mils. Hole diameter is 40mils. Pad diameter is hole
diameter + 15mils. Board thickness is 78mils.
Can you point me to a reference regarding this matter?
Thanks in advance for any assistance.
Regards,
Manoj Viswambharan
Principal Design Engineer
Village Networks, Inc.
[log in to unmask]
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To set a vacation stop for delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------