DESIGNERCOUNCIL Archives

November 2007

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Anderson, Veronika" <[log in to unmask]>
Reply To:
(Designers Council Forum)
Date:
Thu, 29 Nov 2007 12:16:21 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (236 lines)
There is a paragraph 4.1.2 in IPC-2221A, which refers to the Table 4-1.

Veronika Anderson, C.I.D.
Senior Electrical / Mechanical Designer
 
PerkinElmer Optoelectronics
1330 East Cypress St.,
Covina, CA 91724
Phone: (626) 967-9521 X 236
E-mail: [log in to unmask]
 
This email and any attachments thereto may contain private,
confidential, privileged and ITAR controlled material for the sole use
of the intended recipient. Any review, copying, or distribution of this
email (or any attachments thereto) by others is strictly prohibited. If
you are not the intended recipient, please contact the sender
immediately and permanently delete the original and any copies of this
email and any attachments thereto.
 
-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of Jack
Olson
Sent: Thursday, November 29, 2007 8:28 AM
To: [log in to unmask]
Subject: Re: [DC] How to Read a Slash Sheet

Yes, its interesting to me how even after so many years of experience,
something will happen to make me dig deeper, and then question how much
I
really know about a subject.

In this case, I was surprised about the "z-axis" sentence in paragraph
6.3so I also tried to dig a little deeper.
I wondered if maybe the newer draft of IPC-2221B would word it
differently.

and, guess what?

The newest draft DOES make a change here...!

Here is the proposed text:


*6.3 Electrical Clearance *Spacing between conductors on individual
layers
should be maximized whenever

possible. The minimum spacing between conductors, between conductive
patterns, and between conductive

materials (such as conductive markings or mounting hardware) and
conductors
*shall *be in accordance with

Table 6-1, and defined on the master drawing.

For Z-axis spacing considerations, use the dielectric breakdown of the
specific material. The dielectric

breakdown as published in IPC-4101 is based on 0.5 mm thick laminate and
may
not be suitable for thin

cores. It is recommended that lower profile copper foils be used when
thin
core laminates are required;

such laminates are susceptible to violating minimum dielectric
thicknesses
between the copper tooth

structure. This enables tighter control of the dielectric thickness.
*

NOTE: *The designer should be aware that the profile roughness of the
copper
foil determines the minimum

dielectric distance between opposing copper *points* within a thin core
laminate. See also IPC-4101 for

tolerances by class and thickness of core; IPC-4562 for surface
roughness of
copper foil types; and IPC-

6012 for the method to determine minimum *dielectric* thickness.
Designers
should be careful not to use

*minimum* dielectric spacing values to determine overall printed board
thickness.
-=-=-=-

Maybe I "lucked out" by questioning something that is coincidentally
being
addressed by the committee.

I still don't understand specifying the strength only for laminates that
are
.5mm or greater on the slash sheets. Our boards commonly have more than
4
layers, so we would rarely use that value I guess.

There's always more to learn, eh?

thanks for writing back

Jack


.
On 11/29/07, McGlaughlin, Jeffrey A <[log in to unmask]> wrote:
>
> Jack -
>
> Your question got me to thinking, so I did a little research.  Way,
way
> back in time when the Mil specs were king we used MIL-STD-275E as the
> guide for design. In it was a much simpler table for the spacing of
> conductors with only 8 possible classes. This table was for edge to
edge
> spacing only, z-axis spacing was fixed to 3.5mil [89um] minimum. This
> language was carried in to the IPC-D-275 specification, however with
the
> advent of IPC-2221 it changed to include z-axis spacing - I for one
> missed this change until now. I have always used the dielectric
> withstanding numbers from the slash sheet/material data sheet de-rated
> by 1/3-2/3 to determine z axis spacing and have only once in twenty
> years experienced a z-axis punch through short. This short, by the
way,
> was as a result of exceeding the rated voltage output by an order of
> magnitude not as a result of the design.
>
> Have I been doing it wrong for so many years?
>
> Jeffrey McGlaughlin, CID
> Engineering Designer
> Battelle
> 505 King Avenue
> Columbus Ohio 43201-2693
> (614)424-7582 Phone
> (614)458-7582 Fax
>
> -----Original Message-----
> From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of
Jack
> Olson
> Sent: Tuesday, November 27, 2007 6:19 PM
> To: [log in to unmask]
> Subject: Re: [DC] How to Read a Slash Sheet
>
> Well, no one ventured a guess on how to read line 5 of a slash
> sheet, so maybe I will try to ask the question a different way....
>
> What good is it to list a certain amount of dielectric strength on a
> slash sheet, if paragraph 6.3 of IPC-2221A specifies that we use
> Table 6-1 for determining z-axis clearance?
>
> For example, if I need to design for 260V, and Table 6-1 specifies
> an 8mil (.2mm) laminate thickness, that's what I need to use,
> right? So the fact that someone says a material strength is xx
> kilovolts is a moot point once I have been constrained to 8mils
> for 260V.
>
> In my memory no one has ever discussed this subject on any IPC
> listserver, which makes me wonder if I'm asking a valid question.
> Am I mixing terms here?
> Jack
>
>
> On 11/14/07, Jack Olson <[log in to unmask]> wrote:
> >
> > Can someone please help me interpret slash sheets of IPC-4101?
> >
> > We are having some board problems, so I went to look up the voltage
> > breakdown (line 5 in the laminate section)
> > It lists 40kV for laminates over .5mm, thick, but nothing is listed
in
> the
> > column for laminates less than .5mm
> > (Our design has .1mm laminate)
> >
> > What does that 40kV mean, and why is it only given for thicker
> laminates?
> >
>
>
------------------------------------------------------------------------
> ---------
> DesignerCouncil Mail List provided as a free service by IPC using
> LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
> To temporarily stop/(restart) delivery of DesignerCouncil send: SET
> DesignerCouncil NOMAIL/(MAIL)
> Search previous postings at: www.ipc.org > On-Line Resources &
Databases
> > E-mail Archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
> ext.2815
>
------------------------------------------------------------------------
> ---------
>

------------------------------------------------------------------------
---------
DesignerCouncil Mail List provided as a free service by IPC using
LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET
DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
---------

---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------

ATOM RSS1 RSS2