I got a mail from my FAB house to increase the NPTH - copper/t
Hi All,
I got a mail from my FAB house to increase the NPTH - copper/trace clearance from 0.010 inch to 0.015 inch for a NPTH hole with drill size 0.150".When my drill hole is 0.150 inch with offset tolerance of +/- 0.003, i still have 0.004 inch safer value when i use 0.010 inch clearance value. When I questioned the FAB house i got feedback that its their DFM rule for maximizing the production yield.
I am not satisfied with the answer, Can anyone help me understand why NPTH to copper/trace clearance should be much higher?
thanks,
Raj.
__________________________________________________________
Yahoo! India Answers: Share what you know. Learn something new
http://in.answers.yahoo.com/
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|
|
|