In addition to paralene you can try acrylic, silicone, or polyurethane coatings. They all have different advantages under different conditions. Good sources of information are vendor literature from CONAP or HUMISEAL companies or IPC-CC-830 or MIL-I-46058.
Bill Dieffenbacher
Lockheed Martin Control Systems
----------
From: Maquelsa
Sent: Friday, May 23, 1997 7:58 AM
To: [log in to unmask]
Subject: protect circuits.
I am work in hearing aid manufacturing. This miniaturized circuits has
a lot of problems due to humidity. I would like to know what kind of
material I could to use to protect them. I refer to cover the circuit with
a laquer using in other type of circuits.
Thank you.
Job Lima
Audinsa
***************************************************************************
* The mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text.*
***************************************************************************
* If you are having a problem with the DesignerCouncil, please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* The mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text.*
***************************************************************************
* If you are having a problem with the DesignerCouncil, please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|