Subject: | |
From: | |
Reply To: | DesignerCouncil E-Mail Forum. |
Date: | Fri, 12 Jun 1998 13:28:45 -0500 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Just an update. J-STD-001B covers wire stripping and tinning in paragraph 6.1.3;
visual info on stripping is in IPC-A-610 paragraph 3.5.2.2; J-STD-002 addresses now
to accomplish solderability testing and defines acceptable test results.
>>> Lisa Williams <[log in to unmask]> 06/12/98 09:33AM >>>
I believe that J-STD-002, Solderability Tests for Component Leads, Terminations, Lugs
Terminals and Wires, covers the wire stripping & tinning...not sure about the
routing.
J-STD-002 is available through the IPC: $15 members/$30 nonmembers
Call IPC for electronic pricing information.
Lisa Williams
IPC
2215 Sanders Road
Northbrook, IL 60062
URL: www.ipc.org
>>> Joe Reichert <[log in to unmask]> 06/11/98 03:53PM >>>
Good "It's Almost Friday" to everyone!!
Would anyone have any idea where I might
find a spec on wire stripping, wire tinning,
and the routing of wires?
Thanks,
Joe Reichert
:::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::::
Joe Reichert
Lake Shore Cryotronics, Inc.
575 McCorkle Boulevard
Westerville, OH 43082
Voice: 614-891-2243 x238 Fax: 614-818-1605
E-mail: [log in to unmask]
Check out our web site @ http://www.lakeshore.com
################################################################
DesignerCouncil E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE DesignerCouncil <your full name>
To unsubscribe: SIGNOFF DesignerCouncil
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################
################################################################
DesignerCouncil E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE DesignerCouncil <your full name>
To unsubscribe: SIGNOFF DesignerCouncil
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################
################################################################
DesignerCouncil E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE DesignerCouncil <your full name>
To unsubscribe: SIGNOFF DesignerCouncil
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|