CEM-1 or CEM-3 might be a better alternative for high volume consumer
products. FR4 might be cheaper than FR1-FR2 because it is readily
available. The CEM materials are good for punched boards.
----------
From: scotts
Sent: Wednesday, June 11, 1997 11:33 AM
To: designercouncil
Cc: scott.shepard
Subject: FR1 and FR2
Hi,
I've been very lucky to use FR4 or better material. The next batch of
pcb I will layout will be FR2 or FR1 for mass production(1-3000 per
month). I am looking for design rule suggestions that I am not familiar
with or gotchas for these cheap materials. Example min/pref annular ring
on for pads-hole, min/preferred trace width, via placement for epoxy,
etc.
Any help will be appreciated -- thanks in advance,
Scott Shepard
**************************************************************************
*
* The mail list is provided as a service by IPC using SmartList v3.05
*
**************************************************************************
*
* To unsubscribe from this list at any time, send a message to:
*
* [log in to unmask] with <subject: unsubscribe> and no
text.*
**************************************************************************
*
* If you are having a problem with the DesignerCouncil, please contact
*
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]
*
**************************************************************************
*
__________________________________
Scott Buscomb, Senior CAD Designer
[log in to unmask]
voice 770 338-6170
MTCC/Panasonic, Pager Development
1225 Northbrook Pkwy, Ste 2-358
Suwanee, GA USA 30024
__________________________________
***************************************************************************
* The mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text.*
***************************************************************************
* If you are having a problem with the DesignerCouncil, please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|