Hi Rich.

Our Assembly house doesn't like 0603 on the bottom either bridging and
tombstoning..

> -----Original Message-----
> From: DesignerCouncil [mailto:[log in to unmask]]On Behalf Of Rich
> Schutz
> Sent: Wednesday, September 27, 2000 7:20 AM
> To: [log in to unmask]
> Subject: [DC] Wave solder 0603 components
>
>
>  We have concerns of solder bridging occurring when wave
> soldering 0603's. Can
> anyone tell me if they ever done this before?
>
> 1). What were the results ?