> Under the code ENIG
> Finish Electroless nickel 3 micrometers min all 3 classes
> Finish Immersion gold .05 micrometers min all 3 classes
>
>
>
>
> -----Original Message-----
> From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of
> Smith, Donn
> Sent: Wednesday, July 13, 2005 9:35 AM
> To: [log in to unmask]
> Subject: [DC] Plating thickness
>
> I find that my set of IPC-2220 has become outdated (specifically 2221).
> So that I don't have to wait until I can requisition and receive my new
> set, may I impose on someone who already has the new version?
>
> Referencing the Feb 1998 version of that document, Table 4-3 Final
> Finish, Surface Plating Requirements (page 20):
>
> Electroless Nickel 2.5 - 5.0 micrometers (across all three classes)
> Immersion Gold 0.08 - 0.23 micrometers (across all three
> classes)
>
> Here's the question(s): Have either or both of those thicknesses
> changed in the newer version (IPC-2221A)? If so, what are the new
> values?
>
> Thanks very much (in advance)!
>
> Donn
>
> Donn Smith, CID
> Senior PCB Designer
> GARMIN International
> 1200 E. 151st Street
> Olathe, KS 66062
> (913)397-8200
> (913)397-8282 Fax
> [log in to unmask]
> www.garmin.com
>
>
>
> -------------------------
> This e-mail and any attachments may contain confidential material for
> the sole use of the intended recipient. If you are not the intended
> recipient, please be aware that any disclosure, copying, distribution or
> use of this e-mail or any attachment is prohibited. If you have
> received this e-mail in error, please contact the sender and delete all
> copies.
> Thank you for your cooperation
>
> ------------------------------------------------------------------------
> ---------
> DesignerCouncil Mail List provided as a free service by IPC using
> LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with
> following text in the BODY (NOT the subject field): SIGNOFF
> DesignerCouncil.
> To temporarily stop/(restart) delivery of DesignerCouncil send: SET
> DesignerCouncil NOMAIL/(MAIL) Search previous postings at: www.ipc.org >
> On-Line Resources & Databases > E-mail Archives Please visit IPC web
> site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> ------------------------------------------------------------------------
> ---------
>
> --------------------------------------------------------------------------
> -------
> DesignerCouncil Mail List provided as a free service by IPC using LISTSERV
> 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
> To temporarily stop/(restart) delivery of DesignerCouncil send: SET
> DesignerCouncil NOMAIL/(MAIL)
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> --------------------------------------------------------------------------
> -------
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|